Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
51 mm/min; ASTM D638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
Type I; ASTM D638
Flexural Strength 68.9 MPa
9990 psi
13 mm/min; ASTM D790
Flexural Modulus 2.69 GPa
390 ksi
13 mm/min; ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Features Amorphous
Good Moldability
Good Toughness
Forms Pellets
Generic Material ABS
Generic Name Acrylonitrile Butadiene Styrene (ABS)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Appliances
Automotive Applications
Consumer Applications
General Purpose
Industrial Applications
Structural Parts