Mechanical Properties Metric English Comments
Flexural Strength 44.8 MPa
6500 psi
Ohio Carbon Blank OCB AR-06 EDM Grade Graphite
Available in a range of sizes and shapes.
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced
Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Improved stiffnessInfor..
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
PolyOne Stat-Tech™ AS-10CP/000 Acrylonitrile Butadiene Styrene (ABS)  (discontinued **)
Description/Features:AntistaticConductive Carbon Powder FilledInformation provided by PolyOne Corporation.
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
I. Stern HIPS 8 High Impact Polystyrene Injection Grade
Features:Good processing characteristicsComplies with FDA requirements as described in Title 21 CFR 177.1640ApplicationsDisplaysHouse waresStructural FoamInformation provided by I. Stern & Co. Inc.
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
ITW Devcon Metal Repair Wear Resistant Epoxy (WR-2), Dark Grey
Information provided by ITW Devcon
Flexural Strength 44.8 MPa
6500 psi
SGL Carbon Group EK 10 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Flexural Strength 44.8 MPa
6500 psi
SGL Carbon Group EK 2239 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Techmer ES Electrafil® ABS-1200/SD/FR BL ABS
Flexural Strength 44.8 MPa
6500 psi
Max Load; ASTM D790
Spartech PE4325 Reinforced High Density Polyethylene Compound
Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a..
Flexural Strength 44.8 MPa
6500 psi
ASTM D 790
Styrolution PS 5310 HIPS
Excellent ESCRGood ToughnessMatte easily decorated finishInformation provided by Styrolution
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Westlake Plastics Kynar® PVDF CN-P Polyvinylidene Fluoride (conductive)
Carbon-powder-filled, thermally stable, conductive material with consistent resistivities
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Total PSI 625 Polystyrene
Polystyrene 625 is a medium impact polystyrene with balanced physical properties. Thin walled parts with complex runners and gates, run fast and consistently with the easy flow 625. The natural whi..
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Adell RQ-14 Copolymer Polypropylene, 20% Mica Reinforced
Data provided by Adell Plastics, Inc.
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Asahi Kasei Thermylene® F6-10FG-0100 10% Glass Fiber Reinforced, Chemically Coupled
Information provided by Asahi Thermofil
Flexural Strength 44.8 MPa
6500 psi
BCC Products BC 6126 Epoxy Surface Coat/Casting
BC 6126 is a gray, low toxicity, aluminum filled, epoxy surface coat. This thixotropic resin system provides excellent surface duplication along with vertical coverage to 1/16 inch thickness. This h..
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Asahi Kasei Thermofil P-40TC-2767 40% Talc Reinforced, Heat Stabilized
Information provided by Asahi Thermofil