Material Notes:
Features:Good processing characteristicsComplies with FDA requirements as described in Title 21 CFR 177.1640ApplicationsDisplaysHouse waresStructural FoamInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D995
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 24.8 MPa
3600 psi
ASTM D638
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 96.1 °C
205 °F
ASTM D1525
Heat Distortion Temperature 89.4 °C
193 °F
ASTM D648
Flammability, UL94 HB
HB