Material Notes:
Polystyrene 625 is a medium impact polystyrene with balanced physical properties. Thin walled parts with complex runners and gates, run fast and consistently with the easy flow 625. The natural whiteness of 625 allows for brightness of color matches. 625 is the base carrier of choice for concentrate producers.This polymer is utilized in applications such as scale models, toys, house wares, and containers requiring consistency from shot to shot.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 13 g/10 min

@Load 5.00 kg,
Temperature 200 °C
13 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Yield 45 %
45 %
ASTM D638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D638
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Falling Dart Impact 11.3 J
8.33 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 87.8 °C
190 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 92.2 °C
198 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 95 %
95 %
60°; ASTM D523