Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 36.0 MPa | 5220 psi | X direction, Condition A; ASTM D790 |
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowLow Z-axis expansion. Provides reliable plated through holes in multi-layer boardsTight .. |
|||
Flexural Strength | <= 36.0 MPa | <= 5220 psi | ISO 178 |
Polykemi AB POLYelast TPE HJ753 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 36.0 MPa | <= 5220 psi | ISO 178 |
Polykemi AB POLYfill PP CQX8025 R2 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Flexural Strength | <= 36.0 MPa | <= 5220 psi | ISO 178 |
Polykemi AB POLYfill PP EQX10030R UV Polypropylene, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Strength | <= 36.0 MPa | <= 5220 psi | ISO 178 |
Polykemi AB POLYfill PPC TS4030 H Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 36.0 MPa | 5220 psi | 0.1 in/min; ASTM D790 |
Ineos Nova 1983 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Color Stable, Custom colors, UL94 HB at 0.060 for all colorsApplications: Suitable for extrusion or injection molding processes requiring.. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | 0.1 in/min; ASTM D790 |
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app.. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | 2mm/min; ASTM D790 |
Kingfa FRHIPS-100 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mmLow smoking, low halogenExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV or aud.. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific) LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON FX91304 PE LNP* STAT-KON* FX91304 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific) LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Teknor Apex Sinelec CCB2095 Specialty Polystyrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Forms: Pellets Processing Method: Injection MethodInformation Provided by Teknor Ape.. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Teknor Apex Sinpolene TPP2010 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Automotive Applications; Housings Forms: Pellets Process.. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | 3.5% strain; ISO 178 |
Borealis Daplen™ EF267AI Polypropylene TPO Compound Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Polyram RamOfin PPC500 Polypropylene, Flame Retardant Flame retardant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Polyram RamTough RZ309G18 Polycarbonate, 18% Glass Fiber 18% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | 2 mm/min, 4 mm; ISO 178 |
Chi Mei Kibiton® PB-5903 SBC High transparency, high toughness, PS Impact modifier |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ISO 178 |
Eurostar Starpylen HZ 50E3 PP, Injection Molded PRELIMINARY-Starpylen HZ 50E3 is a High Specific Gravity Polypropylene (density 1.5), Injection Molding Resin (also known as HZ50E3)Information provided by Eurostar. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334C40L1 Calcium Reinforced |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334W10L1 Wollastonite Reinforced |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336C10L1 Calcium Reinforced |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336C20L1 Calcium Reinforced |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336C30L1 Calcium Reinforced |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336C40L1 Calcium Reinforced |
|||
Flexural Strength | 36.0 MPa | 5220 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 200 HI4 POM Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | 0.1 in/min; ASTM D790 |
Ineos Nova 8049 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High gloss at 60°=95; at 20°C=90, Improved scuff resistance, Custom colorsApplications: Injection molding, Cost effective replacement for some ABS applications, Excellent for applications where hi.. |
|||
Flexural Strength | 36.0 MPa | 5220 psi | at 3.5% strain; ISO 178 |
Borealis ME268Al Polypropylene Compound, Mineral Filled ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par.. |