Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Homopolymer HP0336C20L1 Calcium Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0336C20L1 Calcium Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
MD; ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Ash 19.7 %
19.7 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ASTM D785
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM D638
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Tensile Modulus 1.500 GPa
217.5 ksi
ASTM D638
Flexural Strength 36.0 MPa
5220 psi
ASTM D790
Flexural Modulus 1.700 GPa
246.5 ksi
ASTM D790
Izod Impact, Notched 0.422 J/cm
0.790 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 58.9 °C
138 °F