Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.
Physical Properties Metric English Comments
Density 4.00 g/cc
0.145 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0089 cm/cm

@Time 86400 sec
0.0089 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0101 cm/cm

@Time 86400 sec
0.0101 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
ISO 527
Tensile Strength, Yield 16.0 MPa
2320 psi
ISO 527
Elongation at Break 2.6 %
2.6 %
ISO 527
Elongation at Yield 1.8 %
1.8 %
ISO 527
Tensile Modulus 6.59 GPa
956 ksi
1 mm/min; ISO 527
Flexural Strength 36.0 MPa
5220 psi
ISO 178
Flexural Modulus 9.58 GPa
1390 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1U
Impact Test 2.00 J
1.48 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved