Mechanical Properties Metric English Comments
Flexural Strength 216 MPa
31300 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Lubricomp DEL34 PC (Europe-Africa-Middle East)
LNP* Lubricomp* DEL34 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP f..
Flexural Strength 216 MPa
31300 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC
LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated.
Flexural Strength 216 MPa
31300 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC (Asia Pacific)
LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Strength 216 MPa

@Temperature 149 °C
31300 psi

@Temperature 300 °F
ASTM D790
Mitsui AURUM® JCL3030 Polyimide, Carbon Fiber Filled  (discontinued **)
AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU..
Flexural Strength 216 MPa

@Temperature 149 °C
31300 psi

@Temperature 300 °F
ASTM D790
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled  (discontinued **)
AURUM JCN3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU..
Flexural Strength 216 MPa
31400 psi
ASTM D790
Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties)
Description:#90 Isophthalic Polyester Resin is perfect for making dimensionally stable polyester molds, corrosive service part fabrication, and as a durable repair material for tank linings. #90 per..
Flexural Strength 216 MPa
31300 psi
ASTM D790
Kolon KOPA® KN333HB40HFBL Hybrid Nylon 66
High flow, dimensionally stableApplications Fans & ShroudsInformation provided by API-Kolon.
Flexural Strength 216 MPa
31300 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI
LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Flexural Strength 216 MPa
31300 psi
ASTM D 790
SABIC Innovative Plastics Valox® VC120 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Strength 216 MPa
31300 psi
ISO 178
SABIC Innovative Plastics LNP Thermocomp EC002E PEI
LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas..
Flexural Strength 216 MPa
31300 psi
ISO 178
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific)
LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac..
Flexural Strength 216 MPa
31300 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled
Good WeatherabilityInformation provided by Samsung Cheil Industries.
Flexural Strength 216 MPa
31300 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® AR-9301 PA, Glass Filled General Purpose
Information provided by Samsung Cheil Industries.
Flexural Strength 216 MPa
31300 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled
Information provided by Samsung Cheil Industries.
Flexural Strength 216 MPa
31300 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® VB-5400G PBT, Glass Filled FR
Information provided by Samsung Cheil Industries.
Flexural Strength 216 MPa
31300 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® AR-9301 PA, Glass Filled General Purpose
Information provided by Samsung Cheil Industries.
Flexural Strength 216 MPa
31300 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled
Good WeatherabilityInformation provided by Samsung Cheil Industries.
Flexural Strength 216 MPa
31300 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled
Information provided by Samsung Cheil Industries.
Flexural Strength 216 MPa
31300 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® VB-5400G PBT, Glass Filled FR
Information provided by Samsung Cheil Industries.
Flexural Strength 216 MPa
31300 psi
ASTM D790
SABIC Innovative Plastics NORYL GTX GTX6801 PPE+PA (Asia Pacific)
PPE+PA, GF 30%
Flexural Strength 216 MPa
31300 psi
Rigidty. Elastic bending fatigue, Longitudinal
CLAL-MSX NICLAFOR® 1000 TD1 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Flexural Strength 216 MPa
31300 psi
2 mm/min; ISO 178
Eurostar Starflam RF0077E PA66, 35% Glass Filled, Injection Molded
Starflam RF0077E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as RF1007Z270)Information provided by Polymer T..
Flexural Strength 216 MPa
31300 psi
ASTM D790
Ashley Polymers Ashlene® 527LD-45LG Nylon 66, 45% Long Glass Fiber Reinforced
Long glass fiber reinforced impact modified Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced r..
Flexural Strength 216 MPa
31300 psi
2.8mm/min; ASTM D790
Asia International Enterprise (Hong Kong) 60G4 Nylon 66, 20% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Flexural Strength 216 MPa
31300 psi
ASTM D790
A. Schulman ComAlloy Hiloy® 716 PPS, Carbon Fiber Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.