Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL GTX GTX6801 PPE+PA (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX GTX6801 PPE+PA (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+PA, GF 30%
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 24.2 g/10 min

@Load 5.00 kg,
Temperature 280 °C
24.2 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 157 MPa
22800 psi
SABIC - Japan Method
Elongation at Break 10 %
10 %
SABIC - Japan Method
Flexural Strength 216 MPa
31300 psi
ASTM D790
Flexural Modulus 8.43 GPa
1220 ksi
ASTM D790
Izod Impact, Notched 0.880 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 230 °C

@Thickness 6.40 mm
446 °F

@Thickness 0.252 in
unannealed; ASTM D648