Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 55.0 MPa @Strain 1.00 %, Temperature 23.0 °C |
7980 psi @Strain 1.00 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Tensile Stress | 55.0 MPa @Strain 4.00 %, Temperature 150 °C |
7980 psi @Strain 4.00 %, Temperature 302 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Tensile Stress | 55.0 MPa @Strain 2.00 %, Temperature 120 °C |
7980 psi @Strain 2.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 55.0 MPa @Strain 3.00 %, Temperature 150 °C |
7980 psi @Strain 3.00 %, Temperature 302 °F |
|
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod.. |
|||
Tensile Stress | 55.0 MPa @Strain 2.00 % |
7980 psi @Strain 2.00 % |
|
Solvay TECHNYL® A 402H1 Natural PA66, DRY Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Tensile Stress | 55.0 MPa @Strain 1.00 %, Temperature 120 °C |
7980 psi @Strain 1.00 %, Temperature 248 °F |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Tensile Stress | 55.0 MPa @Strain 2.10 %, Temperature -40.0 °C |
7980 psi @Strain 2.10 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Tensile Stress | 55.0 MPa @Strain 0.520 %, Temperature 60.0 °C |
7980 psi @Strain 0.520 %, Temperature 140 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Tensile Stress | 55.02 MPa @Strain 2.75 %, Temperature 150 °C |
7980 psi @Strain 2.75 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided .. |
|||
Tensile Stress | 55.0 MPa @Strain 1.00 %, Temperature 40.0 °C |
7980 psi @Strain 1.00 %, Temperature 104 °F |
ISO 527 |
BASF Ultradur B 4300 G4 20% Glass Filled PBT Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 55.0 MPa @Strain 1.80 %, Time 3.60e+7 sec |
7980 psi @Strain 1.80 %, Time 10000 hour |
ISO 899-1 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Tensile Stress | 55.0 MPa @Strain 1.40 %, Time 3.60e+6 sec |
7980 psi @Strain 1.40 %, Time 1000 hour |
ISO 899-1 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Tensile Stress | 55.0 MPa @Strain 1.00 %, Temperature 160 °C |
7980 psi @Strain 1.00 %, Temperature 320 °F |
|
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Tensile Stress | 55.0 MPa @Temperature 200 °C |
7980 psi @Temperature 392 °F |
|
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand .. |
|||
Tensile Stress | 55.0 MPa @Strain 2.00 %, Temperature -40.0 °C |
7980 psi @Strain 2.00 %, Temperature -40.0 °F |
ISO 527 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Tensile Stress | 55.0 MPa @Strain 2.00 %, Time 3.60e+6 sec |
7980 psi @Strain 2.00 %, Time 1000 hour |
60°C; DIN 50014-23/50-2 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |