Polymer Property : Tensile Stress = 55.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 55.0 MPa

@Strain 1.00 %,
Temperature 23.0 °C
7980 psi

@Strain 1.00 %,
Temperature 73.4 °F
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
Tensile Stress 55.0 MPa

@Strain 4.00 %,
Temperature 150 °C
7980 psi

@Strain 4.00 %,
Temperature 302 °F
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
Tensile Stress 55.0 MPa

@Strain 2.00 %,
Temperature 120 °C
7980 psi

@Strain 2.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 55.0 MPa

@Strain 3.00 %,
Temperature 150 °C
7980 psi

@Strain 3.00 %,
Temperature 302 °F
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod..
Tensile Stress 55.0 MPa

@Strain 2.00 %
7980 psi

@Strain 2.00 %
Solvay TECHNYL® A 402H1 Natural PA66, DRY
Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The ..
Tensile Stress 55.0 MPa

@Strain 1.00 %,
Temperature 120 °C
7980 psi

@Strain 1.00 %,
Temperature 248 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 55.0 MPa

@Strain 2.10 %,
Temperature -40.0 °C
7980 psi

@Strain 2.10 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging..
Tensile Stress 55.0 MPa

@Strain 0.520 %,
Temperature 60.0 °C
7980 psi

@Strain 0.520 %,
Temperature 140 °F
ISO 527
DuPont Performance Polymers Rynite® FR543 NC010 PET
Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm..
Tensile Stress 55.0 MPa

@Strain 1.00 %,
Temperature 40.0 °C
7980 psi

@Strain 1.00 %,
Temperature 104 °F
ISO 527
BASF Ultradur B 4300 G4 20% Glass Filled PBT
Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Tensile Stress 55.0 MPa

@Strain 1.80 %,
Time 3.60e+7 sec
7980 psi

@Strain 1.80 %,
Time 10000 hour
ISO 899-1
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM
Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness.
Tensile Stress 55.0 MPa

@Strain 1.40 %,
Time 3.60e+6 sec
7980 psi

@Strain 1.40 %,
Time 1000 hour
ISO 899-1
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM
Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness.
Tensile Stress 55.0 MPa

@Strain 1.00 %,
Temperature 160 °C
7980 psi

@Strain 1.00 %,
Temperature 320 °F
BASF Ultrason S 2010 G6 30% Glass Filled PSU
Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
Tensile Stress 55.0 MPa

@Temperature 200 °C
7980 psi

@Temperature 392 °F
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide
Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand ..
Tensile Stress 55.0 MPa

@Strain 2.00 %,
Temperature -40.0 °C
7980 psi

@Strain 2.00 %,
Temperature -40.0 °F
ISO 527
BASF Ultradur B 4520 PBT
Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade.
Tensile Stress 55.0 MPa

@Strain 2.00 %,
Time 3.60e+6 sec
7980 psi

@Strain 2.00 %,
Time 1000 hour
60°C; DIN 50014-23/50-2
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..