Mechanical Properties Metric English Comments
Tensile Stress 2.56 MPa

@Strain 300 %
371 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P2655 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.56 MPa

@Strain 50.0 %
371 psi

@Strain 50.0 %
Average; ASTM D412 Method A
Seals Eastern 5794 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..
Tensile Stress 2.56 MPa

@Strain 0.200 %,
Temperature 100 °C
371 psi

@Strain 0.200 %,
Temperature 212 °F
ISO 11403-1/-2
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer
Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided ..
Tensile Stress 2.56 MPa

@Strain 129.46 %,
Temperature 120 °C
371 psi

@Strain 129.46 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 2.56 MPa

@Strain 26.22 %,
Temperature 120 °C
371 psi

@Strain 26.22 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..