Material Notes:
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInformation from Alliance Polymers & Services, Distributor of Nantong Elastomer Technology Co.Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 55

@Time 10.0 sec
55

@Time 0.00278 hour
ASTM D2240
Tensile Stress 1.93 MPa

@Strain 100 %
280 psi

@Strain 100 %
ASTM D412
2.56 MPa

@Strain 300 %
371 psi

@Strain 300 %
ASTM D412
Tensile Strength, Yield 3.55 MPa
515 psi
ASTM D412
Elongation at Break 610 %
610 %
ASTM D412
Tear Strength 20.3 kN/m
116 pli
ASTM D624