Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.45 MPa @Strain 300 % |
1370 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® A9885H TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 9.44 MPa @Strain 0.100 %, Temperature -40.0 °C |
1370 psi @Strain 0.100 %, Temperature -40.0 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® LW9330 BK851 PBT
(Unverified Data**) Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Tensile Stress | 9.45 MPa @Strain 133.22 %, Temperature 100 °C |
1370 psi @Strain 133.22 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.42 MPa @Strain 133.91 %, Temperature 120 °C |
1370 psi @Strain 133.91 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.44 MPa @Strain 88.76 %, Temperature 100 °C |
1370 psi @Strain 88.76 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.45 MPa @Strain 8.11 %, Temperature 40.0 °C |
1370 psi @Strain 8.11 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.443 MPa @Strain 0.546765 %, Temperature 160 °C |
1370 psi @Strain 0.546765 %, Temperature 320 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |