Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.45 MPa @Strain 300 % |
1370 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® A9885H TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 9.45 MPa @Strain 133.22 %, Temperature 100 °C |
1370 psi @Strain 133.22 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.45 MPa @Strain 8.11 %, Temperature 40.0 °C |
1370 psi @Strain 8.11 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |