Braskem CP 284R HECO Polypropylene Heterophasic Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem CP 284R HECO Polypropylene Heterophasic Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CP 284R is a heterophasic copolymer designed for injection molding of pails and containers with excellent stiffness/impact strength balance. This resin also exhibits excellent productivity and processability. Its applications include: good stiffness parts, household, and industrial pails.
Physical Properties Metric English Comments
Density 0.895 g/cc
0.0323 lb/in³
ASTM-D792
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 62
62
ASTM-D785
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM-D638
Elongation at Yield 5.0 %
5.0 %
ASTM-D638
Flexural Modulus, 1% Secant 1100 MPa
160000 psi
ASTM-D790
Izod Impact, Notched 0.690 J/cm

@Temperature -20.0 °C
1.29 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ASTM-D648
Vicat Softening Point 146 °C

@Load 1.02 kg
295 °F

@Load 2.25 lb
ASTM-D1525