Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.690 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87570 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -30.0 °C |
1.29 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -30.0 °C |
1.29 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem AUT230M PEI Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are .. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem AUT230M PEI (Europe-Africa-Middle East) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem XH6050F PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was .. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar 5011 Copolyester Eastar Copolyester 5011 is a glycol modified polyethylene terephthalate(PET). The modification is made by adding a second glycol, cyclohexanedimethanol (CHDM) during the polymerization stages. The s.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -40.0 °C |
1.29 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar DN001HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -40.0 °C |
1.29 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar DN004HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN004HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar MN200 Copolyester Eastar Copolyester MN200 is an amorphous copolyester with excellent flow characteristics as well as radiation resistance and chemical resistance.Applications/UsesMedical |
|||
Izod Impact, Notched | 0.690 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® X5403 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.690 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® X5403 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -20.0 °C |
1.29 ft-lb/in @Temperature -4.00 °F |
ASTM-D256 |
Braskem CP 284R HECO Polypropylene Heterophasic Copolymer CP 284R is a heterophasic copolymer designed for injection molding of pails and containers with excellent stiffness/impact strength balance. This resin also exhibits excellent productivity and proce.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -40.0 °C |
1.29 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |