Techmer ES Electrablend® PA6/6 03002 A MB Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled , Nylon 66, Conductive , Nylon 66, Heat Stabilized , Nylon 66, Impact Grade
Manufacturer Techmer ES
Trade Name Electrablend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® PA6/6 03002 A MB Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement/Unspecified Filler/Reinfor.Additive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact Modified and Heat StabilizedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Water Absorption 0.90 %

@Time 86400 sec
0.90 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Thickness 3.17 mm
0.012 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength, Yield 84.1 MPa
12200 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 3.62 GPa
525 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.00 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
1.49 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
2.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 79.2 µm/m-°C
44.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 252 °C
485 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 10 - 1000 ohm-cm
10 - 1000 ohm-cm
ASTM D257
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257