Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.750 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.750 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.41 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87560 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 0.750 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
1.41 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ISO 180/4A
Polimeri Europa Sinkral® PD D 232/M4 ABS Resin
Special very low gloss extrusion / co-extrusion grade, with good flow.Applications: Sinkral PD D 232/M4 is widely used in extrusion / co-extrusion of foils, when a very high matte appearance is req..
Izod Impact, Notched 0.750 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
1.41 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PBT 1455
PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel..
Izod Impact, Notched 0.750 J/cm

@Temperature -30.0 °C
1.41 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP ..
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWE280 ASA
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East)
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 0.750 J/cm

@Temperature -40.0 °C
1.41 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Eastar 5445 PCTG Copolyester, Injection Molded  (discontinued **)
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t..
Izod Impact, Notched 0.750 J/cm

@Temperature -20.0 °C
1.41 ft-lb/in

@Temperature -4.00 °F
ASTM D256
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific)
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.750 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
1.41 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PPE 1461  (discontinued **)
PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric..
Izod Impact, Notched 0.750 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
1.41 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ISO 180/4A
Polimeri Europa Sinkral® D 232/M3 ABS Resin  (discontinued **)
Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr..
Izod Impact, Notched 0.750 J/cm

@Temperature -20.0 °C
1.41 ft-lb/in

@Temperature -4.00 °F
ASTM D256
LATI LASULF Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LATI LASULF Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
50%RH; ASTM D256
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® TY-791HT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.750 J/cm

@Temperature -40.0 °C
1.41 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Tenite 307E0V16310 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Izod Impact, Notched 0.750 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
1.41 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Diamond Polymers Centrex® 814 General Purpose Injection Molding Grade
Centrex 814 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and processing perfor..
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Carmel Olefins CAPILENE® SW 75 AV Polypropylene Impact Copolymer
Description: CAPILENE® SW 75 AV is a high melt flow rate, controlled rheology impact copolymer for injection molding. CAPILENE® SW 75 AV is nucleated with antistatic additivation. It is characte..
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)  (discontinued **)
Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f..
Izod Impact, Notched 0.750 J/cm

@Temperature -40.0 °C
1.41 ft-lb/in

@Temperature -40.0 °F
ASTM D256
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Izod Impact, Notched 0.750 J/cm

@Temperature -40.0 °C
1.41 ft-lb/in

@Temperature -40.0 °F
ASTM D256
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)  (discontinued **)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Izod Impact, Notched 0.750 J/cm

@Temperature -20.0 °C
1.41 ft-lb/in

@Temperature -4.00 °F
ASTM D256
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)  (discontinued **)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)  (discontinued **)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM D256
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved