Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 1.31 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00900 GPa
1.31 ksi
0.025" extruded film; DIN 53504
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester
Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti..
300% Modulus 0.00900 GPa
1.31 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials Pearlthane® D91T80 Thermoplastic Polyurethane
Type : Pearlthane® D91T80 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties...
300% Modulus 0.00900 GPa
1.31 ksi
DIN 53504
Lubrizol ESTANE® T5090 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412
UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1180 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-2185 Polycaprolactone Based TPU
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412; ASTM D638
Lubrizol Estane® 58610 Thermoplastic Polyurethane
Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee..
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1680AB Polyester Based TPU
Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l..
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412/D638
Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane
Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance, and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin ..
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D638
ELASTO UK Dryflex® 420401S SBS Based Material, 40D Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D638
ELASTO UK Dryflex® 422401S SBS Based Material, 40D Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00900 GPa
1.31 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4640 General Purpose Compound
FormulationNordel® IP 4640
300% Modulus 0.00900 GPa
1.31 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4770P Dense Extruded Profile
FormulationNordel® IP 4770P
300% Modulus 0.00900 GPa
1.31 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4770R Dense Extruded Profile
FormulationNordel® IP 4770R
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412/D638
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane
Features: It has the highest heat resistance of any Estane TPU resin used in adhesives. Supplied as pale amber granules, it is soluble in THF or THF/MEK blends. Higher heat resistance, tensile and b..
300% Modulus 0.00900 GPa
1.31 ksi
DIN 53504
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.00900 GPa
1.31 ksi
DIN 53504
Lubrizol ESTANE® 58214 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.00900 GPa
1.31 ksi
DIN 53504
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Copyright © lookpolymers.com All Rights Reserved