Lubrizol Advanced Materials Pearlthane® D91T80 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlthane® D91T80 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type : Pearlthane® D91T80 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties.Information provided by Merquinsa
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
ISO 868
Tensile Strength 35.03 MPa
5080 psi
ISO 527-2/5A/500
Elongation at Break 700 %
700 %
ISO 527-2/5A/500
50% Modulus 0.00400 GPa
0.580 ksi
ISO 527-2/5A/500
100% Modulus 0.00400 GPa
0.580 ksi
ISO 527-2/5A/500
300% Modulus 0.00900 GPa
1.31 ksi
ISO 527-2/5A/500
Tear Strength 82.0 kN/m
468 pli
ISO 34-1B
Abrasion 30
30
[mm<sup>3</sup>]; ISO 4649-A
Thermal Properties Metric English Comments
Vicat Softening Point 61.0 °C
142 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Nozzle Temperature 210 °C
410 °F
Zone 1 170 °C
338 °F
Zone 2 170 °C
338 °F
Zone 3 175 °C
347 °F
Zone 4 175 °C
347 °F
Dry Time 3.00 hour

@Temperature 80.0 °C
3.00 hour

@Temperature 176 °F
Users viewing this material also viewed the following: