Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® 58610 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® 58610 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, sheet, coated fabric and laminations.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
ASTM D2240
74

@Temperature 70.0 °C
74

@Temperature 158 °F
6 weeks, Heat Resistance
75

@Temperature 100 °C
75

@Temperature 212 °F
10 weeks, Heat Resistance
75

@Temperature 23.0 °C
75

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Shelf
85

@Temperature 23.0 °C
85

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Arizona
85

@Temperature 23.0 °C
85

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Florida
85

@Temperature 23.0 °C
85

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Ohio
85

@Temperature 23.0 °C
85

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Shelf
85

@Temperature 23.0 °C
85

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Florida
89

@Temperature 23.0 °C
89

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Ohio
89

@Temperature 23.0 °C
89

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Arizona
Tensile Strength 4.05 MPa

@Temperature 70.0 °C
587 psi

@Temperature 158 °F
6 weeks, Heat Resistance
5.79 MPa

@Temperature 23.0 °C
840 psi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Florida
6.95 MPa

@Temperature 23.0 °C
1010 psi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Arizona
8.11 MPa

@Temperature 23.0 °C
1180 psi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Ohio
11.58 MPa

@Temperature 23.0 °C
1680 psi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Florida
26.63 MPa

@Temperature 100 °C
3862 psi

@Temperature 212 °F
10 weeks, Heat Resistance
32.42 MPa

@Temperature 23.0 °C
4702 psi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Arizona
41.69 MPa

@Temperature 23.0 °C
6047 psi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Ohio
59.06 MPa

@Temperature 23.0 °C
8566 psi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Shelf
59.06 MPa

@Temperature 23.0 °C
8566 psi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Shelf
Tensile Strength, Ultimate 57.9 MPa
8400 psi
ASTM D412; ASTM D638
Elongation at Break 600 %
600 %
ASTM D412; ASTM D638
222 %

@Temperature 23.0 °C
222 %

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Florida
300 %

@Temperature 23.0 °C
300 %

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Arizona
420 %

@Temperature 23.0 °C
420 %

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Ohio
624 %

@Temperature 23.0 °C
624 %

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Florida
630 %

@Temperature 23.0 °C
630 %

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Shelf
654 %

@Temperature 23.0 °C
654 %

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Shelf
690 %

@Temperature 100 °C
690 %

@Temperature 212 °F
10 weeks, Heat Resistance
714 %

@Temperature 23.0 °C
714 %

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Ohio
720 %

@Temperature 23.0 °C
720 %

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Arizona
1080 %

@Temperature 70.0 °C
1080 %

@Temperature 158 °F
6 weeks, Heat Resistance
100% Modulus 0.00610 GPa
0.885 ksi
ASTM D412; ASTM D638
0.00370 GPa

@Temperature 70.0 °C
0.537 ksi

@Temperature 158 °F
6 weeks, Heat Resistance
0.00400 GPa

@Temperature 100 °C
0.580 ksi

@Temperature 212 °F
10 weeks, Heat Resistance
0.00410 GPa

@Temperature 23.0 °C
0.595 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Arizona
0.00440 GPa

@Temperature 23.0 °C
0.638 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Florida
0.00570 GPa

@Temperature 23.0 °C
0.827 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Florida
0.00580 GPa

@Temperature 23.0 °C
0.841 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Arizona
0.00580 GPa

@Temperature 23.0 °C
0.841 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Ohio
0.00620 GPa

@Temperature 23.0 °C
0.899 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Shelf
0.00620 GPa

@Temperature 23.0 °C
0.899 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Ohio
0.00670 GPa

@Temperature 23.0 °C
0.972 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Shelf
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412; ASTM D638
0.00250 GPa

@Temperature 23.0 °C
0.363 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Ohio
0.00260 GPa

@Temperature 100 °C
0.377 ksi

@Temperature 212 °F
10 weeks, Heat Resistance
0.00260 GPa

@Temperature 23.0 °C
0.377 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Florida
0.00320 GPa

@Temperature 23.0 °C
0.464 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Arizona
0.00350 GPa

@Temperature 23.0 °C
0.508 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Ohio
0.00370 GPa

@Temperature 23.0 °C
0.537 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Shelf
0.00380 GPa

@Temperature 23.0 °C
0.551 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Shelf
Flexural Stiffness 6.40 MPa

@Temperature 23.0 °C
928 psi

@Temperature 73.4 °F
ASTM D474
Taber Abrasion, mg/1000 Cycles 15

@Load 1.00 kg
15

@Load 2.20 lb
H-18 wheel; ASTM D1044
Thermal Properties Metric English Comments
Vicat Softening Point 61.0 °C
142 °F
ASTM D1525
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved