Dow Nordel® IP 4770R Dense Extruded Profile

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dow Chemical
Trade Name Nordel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Nordel® IP 4770R Dense Extruded Profile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormulationNordel® IP 4770R
Physical Properties Metric English Comments
Density 1.185 g/cc
0.04281 lb/in³
Mooney Viscosity 47

@Temperature 100 °C
47

@Temperature 212 °F
ML 1 + 4
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 10.4 MPa
1510 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 446 %
446 %
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00380 GPa
0.551 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 0.00750 GPa
1.09 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.00900 GPa
1.31 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 88 %

@Temperature 125 °C
88 %

@Temperature 257 °F
Pellets cured MDR t'95 + 15 min, 70 hr; Method B