Material Notes:
Description: Kraton A1535 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 57%. It is supplied from North America in the physical form identified: Kraton A1535 HU - supplied as an undusted powderKraton A1535 HS - supplied as a dusted powderRegion: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton A1535 H is used as a base material for compound formulations and as a modifier of thermoplastics. The inherent stability of the mid block suggests the use of this product in applications that must withstand weathering and high processing temperatures.Applications: Compounding and Personal HygieneInformation provided by Kraton®
Physical Properties Metric English Comments
Volatiles <= 1.0 %
<= 1.0 %
KM 04
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 83

@Time 10.0 sec
83

@Time 0.00278 hour
ASTM D2240
Tensile Strength 27.6 MPa
4000 psi
Measured on solution cast film from toluene; BAM 1245
Elongation at Break >= 600 %
>= 600 %
Measured on solution cast film from toluene; BAM 1245
300% Modulus 0.00793 GPa
1.15 ksi
Measured on solution cast film from toluene; BAM 1245
Descriptive Properties Value Comments
Content Non-staining phenolic antioxidant
0.03-0.1%, KM 08
Polystyrene
56.3-60.3%, Measured on the polymer before hydrogenation, KM 03
Total Extractables
<1.6%, KM 05