FormulationNordel® IP 4570
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Mooney Viscosity 64

@Temperature 100 °C
64

@Temperature 212 °F
ML 1 + 4
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 9.30 MPa
1350 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 425 %
425 %
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00330 GPa
0.479 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.00790 GPa
1.15 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 37.1 kN/m
212 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 75 %

@Temperature 100 °C
75 %

@Temperature 212 °F
Pellets cured MDR TC95 + 15 min at 160°C, 22 hr at 100°C; Method B
Thermal Properties Metric English Comments
Brittleness Temperature -43.0 °C
-45.4 °F
Temperature Retraction, TR-10