Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.00 - 7.50 GPa @Temperature 60.0 - 90.0 °C |
870 - 1090 ksi @Temperature 140 - 194 °F |
Average value: 6.75 GPa Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Modulus of Elasticity | 2.16 - 7.50 GPa | 313 - 1090 ksi | Average value: 3.63 GPa Grade Count:66 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Modulus of Elasticity | 6.20 - 7.50 GPa @Temperature 60.0 - 120 °C |
899 - 1090 ksi @Temperature 140 - 248 °F |
Average value: 6.90 GPa Grade Count:1 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Modulus of Elasticity | 2.76 - 7.50 GPa | 400 - 1090 ksi | Average value: 4.12 GPa Grade Count:4 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Modulus of Elasticity | 2.21 - 7.50 GPa | 321 - 1090 ksi | Average value: 3.99 GPa Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |