Mechanical Properties Metric English Comments
Modulus of Elasticity 6.20 - 16.7 GPa
899 - 2420 ksi
Average value: 11.1 GPa Grade Count:11
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Modulus of Elasticity 6.20 - 7.50 GPa

@Temperature 60.0 - 120 °C
899 - 1090 ksi

@Temperature 140 - 248 °F
Average value: 6.90 GPa Grade Count:1
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Modulus of Elasticity 6.20 GPa
899 ksi
ISO 527
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Conditioned)
Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Modulus of Elasticity 6.20 GPa
899 ksi
ISO 527
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Conditioned)
Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Modulus of Elasticity 6.20 GPa
899 ksi
ISO 527-1/-2
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Modulus of Elasticity 6.20 GPa
899 ksi
ISO 527-1/-2
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Modulus of Elasticity 6.20 GPa
899 ksi
ISO 527
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Conditioned)
Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade.
Modulus of Elasticity 6.20 GPa
899 ksi
Conditioned; ISO 178
Addiplast Addinyl B2 V40 Nylon 6, 40% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Modulus of Elasticity 6.20 GPa
899 ksi
Conditioned; ISO 178
Addiplast Addinyl B2 ZV40 Nylon 6, 40% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.