Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.90 - 13.1 GPa | 1000 - 1900 ksi | Average value: 10.7 GPa Grade Count:5 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Modulus of Elasticity | 6.90 - 8.27 GPa | 1000 - 1200 ksi | Average value: 7.70 GPa Grade Count:6 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Modulus of Elasticity | 6.90 - 26.9 GPa | 1000 - 3900 ksi | Average value: 15.3 GPa Grade Count:15 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Modulus of Elasticity | 6.90 GPa | 1000 ksi | ASTM D638 |
Toyobo T-423 Nylon, Mineral-Reinforced Key Feature: High heat distortion and good toughness, good surfaceInformation provided by Toyobo Co., Ltd |
|||
Modulus of Elasticity | 6.90 GPa | 1000 ksi | ISO 527-2 |
BASF Ultradur B 4300 G4 High Speed Unc. 20% Glass Filled PBT Ultradur B 4300 G4 High Speed Unc. is a high flow, fast cycling with low warpage, 20% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap.. |
|||
Modulus of Elasticity | 6.90 GPa | 1000 ksi | ISO 527-2 |
BASF Ultradur S 4090 G4 20% Glass Filled PBT Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio.. |
|||
Modulus of Elasticity | 6.90 GPa | 1000 ksi | ISO 527-2 |
BASF Ultradur S 4090 G4 High Speed Unc. 20% Glass Filled PBT Ultradur S 4090 G4 High Speed Unc. is a high flow, fast cycling with low warpage, 20% glass filled injection molding PBT for industrial parts, rigid tough and dimensional stable applications. |
|||
Modulus of Elasticity | 6.90 GPa | 1000 ksi | GB/T 1040 |
Beijing Evergrow Resources Glass Filled Nylon Information provided by Beijing Evergrow Resources. |
|||
Modulus of Elasticity | 6.90 - 17.0 GPa | 1000 - 2470 ksi | Average value: 12.9 GPa Grade Count:18 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |