Mechanical Properties Metric English Comments
Modulus of Elasticity 6.90 - 26.9 GPa
1000 - 3900 ksi
Average value: 15.3 GPa Grade Count:15
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..