Mechanical Properties Metric English Comments
Modulus of Elasticity 14.0 - 17.0 GPa
2030 - 2470 ksi
Injection; ISO 527
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Modulus of Elasticity 1.60 - 17.0 GPa
232 - 2470 ksi
Average value: 3.03 GPa Grade Count:30
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Modulus of Elasticity 1.10 - 17.0 GPa

@Temperature 60.0 - 175 °C
160 - 2470 ksi

@Temperature 140 - 347 °F
Average value: 10.4 GPa Grade Count:5
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Modulus of Elasticity 4.00 - 17.0 GPa
580 - 2470 ksi
Average value: 9.55 GPa Grade Count:8
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..
Modulus of Elasticity 3.40 - 17.0 GPa
493 - 2470 ksi
Average value: 8.25 GPa Grade Count:10
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Modulus of Elasticity 3.90 - 17.0 GPa
566 - 2470 ksi
Average value: 9.07 GPa Grade Count:100
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Modulus of Elasticity 6.90 - 17.0 GPa
1000 - 2470 ksi
Average value: 12.9 GPa Grade Count:18
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..