Mechanical Properties Metric English Comments
Modulus of Elasticity 128 GPa
18500 ksi
Materion ToughMet® T3 AT110 (OD≥4")
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Modulus of Elasticity 128 GPa
18500 ksi
Materion ToughMet® T3 AT120 (OD≥4")
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Modulus of Elasticity 128 GPa
18500 ksi
Materion ToughMet® T3 AT120 (OD
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Modulus of Elasticity 128 GPa
18500 ksi
Materion ToughMet® T3 AT90 (OD≥4")
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Modulus of Elasticity 128 GPa
18500 ksi
Materion ToughMet® T3 CA
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Modulus of Elasticity 128 GPa
18500 ksi
Materion ToughMet® T3 CX105 (OD≥4")
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Modulus of Elasticity 128 GPa

@Temperature 1000 °C
18600 ksi

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Modulus of Elasticity 128 GPa

@Temperature 1000 °C
18600 ksi

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Modulus of Elasticity 128 GPa

@Temperature 1000 °C
18600 ksi

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Modulus of Elasticity 128 GPa

@Temperature 1000 °C
18600 ksi

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Modulus of Elasticity 128 GPa

@Temperature 1000 °C
18600 ksi

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Modulus of Elasticity 128 GPa
18500 ksi
Materion ToughMet® T3 CX90
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Modulus of Elasticity 128 GPa

@Temperature 1000 °C
18600 ksi

@Temperature 1830 °F
Haynes HR-120® alloy, solution heat-treated plate
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Modulus of Elasticity 128 GPa
18500 ksi
Schmolz + Bickenbach MoldMAX® V Copper Alloy
Description: Brush Wellman’s MoldMAX® V (MMV) is a high conductivity, moderately high strength, copper nickel silicon chromium alloy. Applications include injection mold and blow mold cores ..
Modulus of Elasticity 128 GPa
18600 ksi
Typical
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Annealed Sheet/Plate & Billet/Bar
Low Cost, Multipurpose Alloy. Tensile property data below for Annealed Sheet/Plate & Billet/Bar.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wit..
Modulus of Elasticity 128 GPa
18600 ksi
Typical
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Forged
Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wi..
Modulus of Elasticity 128 GPa
18600 ksi
CMW® 73 Copper Alloy
CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w..
Modulus of Elasticity 128 GPa
18600 ksi
Ultrasonic
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2)
Te value is 670°C. Hasselman Thermal Shock value is 800 K.Data provided by CeramTec North America.
Modulus of Elasticity 128 GPa
18500 ksi
Materion ToughMet® T3 AT110 (OD
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin..
Modulus of Elasticity 128 GPa
18500 ksi
Materion ToughMet® T3 AT90 (OD
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin..
Modulus of Elasticity 128 GPa
18500 ksi
Materion ToughMet® T3 CX105 (OD
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin..
Modulus of Elasticity 128 GPa
18600 ksi
Typical
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA
Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Alpha-Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, ..