Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 128 GPa | 18500 ksi | |
Materion ToughMet® T3 AT110 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Modulus of Elasticity | 128 GPa | 18500 ksi | |
Materion ToughMet® T3 AT120 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Modulus of Elasticity | 128 GPa | 18500 ksi | |
Materion ToughMet® T3 AT120 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Modulus of Elasticity | 128 GPa | 18500 ksi | |
Materion ToughMet® T3 AT90 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Modulus of Elasticity | 128 GPa | 18500 ksi | |
Materion ToughMet® T3 CA ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Modulus of Elasticity | 128 GPa | 18500 ksi | |
Materion ToughMet® T3 CX105 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Modulus of Elasticity | 128 GPa | 18500 ksi | |
Materion ToughMet® T3 CX90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Modulus of Elasticity | 128 GPa | 18500 ksi | |
Schmolz + Bickenbach MoldMAX® V Copper Alloy Description: Brush Wellman’s MoldMAX® V (MMV) is a high conductivity, moderately high strength, copper nickel silicon chromium alloy. Applications include injection mold and blow mold cores .. |
|||
Modulus of Elasticity | 128 GPa | 18500 ksi | |
Materion ToughMet® T3 AT110 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |
|||
Modulus of Elasticity | 128 GPa | 18500 ksi | |
Materion ToughMet® T3 AT90 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |
|||
Modulus of Elasticity | 128 GPa | 18500 ksi | |
Materion ToughMet® T3 CX105 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |