Polymer Property : Modulus of Elasticity = 15000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 103 GPa
15000 ksi
H.C. Starck Pure Niobium (Columbium)
Applications: NRC® niobium metal is produced from electron beam melted ingots. Grain Stabilized Niobium (GSNb) is made by EB and VAR melting. Both materials are malleable, weldable, machineabl..
Modulus of Elasticity 103 GPa

@Temperature 299 °C
15000 ksi

@Temperature 570 °F
Bohler-Uddeholm BeCu Alloy 172 Mold Material
Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha..
Modulus of Elasticity 103 GPa

@Temperature 600 °C
15000 ksi

@Temperature 1110 °F
Latrobe Magnadie - RF Modified Premium H-13 Hot Work Die Steel
Magnadie-RF is a premium quality 5% chromium hot work die steel. The chemistry of Magnadie-RF steel is a modification of the premium quality H-13 chemistry. Magnadie-RF steel is designed for incre..