Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 103 - 110 GPa | 14900 - 16000 ksi | Typical |
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 538°C High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
Modulus of Elasticity | 105 - 110 GPa | 15200 - 16000 ksi | Typical |
TIMET TIMETAL® 679 (Ti-11Sn-5Zr-2.25Al-1Mo-0.2Si) Titanium Alloy; Quenched & Aged High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: USA Aerospace: AMS 4974.Features: TIMETAL 679 has excellent tensile strength and is creep resistant up to 450°C. It i.. |