Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 2700 MPa

@Temperature 23.0 °C
392000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer
Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a..
Tensile Creep Modulus, 1 hour 2700 MPa

@Temperature 23.0 °C
392000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer
Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro..
Tensile Creep Modulus, 1 hour 2700 MPa
392000 psi
Arkema Group Orgalloy® RS 6015 EST Nylon 6 Alloy, 18% Glass Fiber (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties...
Tensile Creep Modulus, 1 hour 2700 MPa
392000 psi
Arkema Group Altuglas® GR 7E LIL Acrylic
ALTUGLAS GR 7E LIL is an injection molding grade with excellent balance between mechanical, thermal and optical properties.Key features : easy processing and demolding improved chemical resistance ..
Tensile Creep Modulus, 1 hour 2700 MPa
392000 psi
Arkema Group Altuglas® 84 L Acrylic-Styrene Copolymer
ALTUGLAS 84 L is a new type of acrylic polymer produced by ATOHAAS which increases the range of material for injection molding applications. ALTUGLAS 84 L is a styrene methylmethacrylate copolymer s..
Tensile Creep Modulus, 1 hour 2700 MPa
392000 psi
Arkema Group Oroglas® V 044 Acrylic, Extrusion Grade  (discontinued **)
OROGLAS V 044 is an extrusion grade offering good compromise between physical properties and thermal resistance.OROGLAS V 044 is recommended for extrusion of profiles, tubes and sheets.ISO data prov..
Tensile Creep Modulus, 1 hour 2700 MPa
392000 psi
Arkema Group Oroglas® V 045 Acrylic, Extrusion Grade  (discontinued **)
OROGLAS V 045 is a lubricated extrusion grade offering good combination of physical and optical properties.OROGLAS V 045 provides easy processing behavior.OROGLAS V 045 is recommended for extrusion..
Tensile Creep Modulus, 1 hour 2700 MPa
392000 psi
Arkema Group Oroglas® V 825 HID Acrylic, UV, Heat Resistant  (discontinued **)
OROGLAS HID is an acrylic resin formulated to withstand continuous exposure to high intensity discharge ( HID ) sources up to 90°c.Above 80°c, OROGLAS V 825 HID resin retains its original appearan..
Tensile Creep Modulus, 1 hour 2700 MPa
392000 psi
Arkema Group Oroglas® V 825 T Acrylic  (discontinued **)
OROGLAS V 825 T exhibits an excellent balance of properties including superior thermal resistance with an easy processing behavior.OROGLAS V 825 T is then the material of choice for automotive appli..
Tensile Creep Modulus, 1 hour 2700 MPa
392000 psi
Arkema Group Oroglas® V 920 Acrylic, Injection Molding Grade  (discontinued **)
OROGLAS V 920 is an injection molding grade with a good balance of properties :Superior flow with medium thermal resistance.The processing of OROGLAS V 920 is easy in terms of injection molding, mo..
Tensile Creep Modulus, 1 hour 2700 MPa
392000 psi
Arkema Group Oroglas® V 920 T Acrylic, Injection Molding Grade  (discontinued **)
OROGLAS V 920 T is an injection molding grade with an improved thermal resistance HDT A ( 1.82 MPa ) = 96°c without any adverse effect on mechanical and optical properties.The processing of OROGLAS..
Tensile Creep Modulus, 1 hour 2700 MPa

@Temperature 23.0 °C
392000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the..