Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.00414 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D412
S&E Specialty Polymers GTPE-2203G1 PVC
Application: RoHS compliant, 105° C, flexible, oil resistant TPE jacketing material with extremely good low temperature properties.Information provided by S&E Specialty Polymers
100% Modulus 0.00414 GPa
0.600 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D412
Mearthane Durethaneâ„¢ S DS-280A Solid Polyurethane Elastomer
TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
100% Modulus 0.00414 GPa
0.600 ksi
Elastomer Engineering E558 Polyurethane
A specially formulated polyester-based urethane for use in abrasion resistance. At use now in mining, grain handling, and gravel conveying applications. Information provided by Elastomer Engineerin..
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D412
Lubrizol Estane® ALR E77A-V Thermoplastic Polyurethane
Type: Estane® ALR E77A-V is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corp..
100% Modulus 0.00414 GPa
0.600 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00414 GPa
0.600 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Zinc Stearate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 8078NL Thermoplastic Elastomer
Elastocon® 8078NL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a scratch and mar resistant surface finish. Elastocon® 8078NL is FDA c..
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D638
Colorite Polymers 6033 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D-638
Axiall 59996J Moldings & Extrusions Flexible PVC
Injection and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D-638
Axiall 8640 Moldings & Extrusions Flexible PVC
General purpose extrusion compound for weatherstrips and tubings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D-638
Axiall 8642 Moldings & Extrusions Flexible PVC
General purpose, fungus resistant extrusion and molding compound recommended for weatherstrips and tubings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D-638
Axiall 8670 Moldings & Extrusions Flexible PVC
General purpose extrusion compound recommended for use in weatherstrips and extruded tubing.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 3065 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00414 GPa
0.600 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2176 Fluoroelastomer
Composition: di-polymer of vinylidene fluoride and hexafluoropropyleneAbility for fast cure cycles with excellent processing safetyMedium viscosityProcess targets: compression and transfer molding, ..
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D-638
Axiall 11600 Wire & Cable Flexible PVC
Clear, non-staining speaker wire insulation and general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D-638
Axiall 16640 Wire & Cable Flexible PVC
Matte finish battery booster cable jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D-638
Axiall 6702 Moldings & Extrusions Flexible PVC
An expandable, low gravity, injection molding compound specifically developed for footwear applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00414 GPa
0.600 ksi
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2211 Fluoroelastomer
Dyneon FC 2211 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The "dry" ingre..
100% Modulus 0.00414 GPa
0.600 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Zinc Stearate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D638
Colorite Polymers 6000 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D638
Colorite Polymers 6742A General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D-638
Axiall 18650 Moldings & Extrusions Flexible PVC
General purpose compound recommended for 105C applications. Well suited for 105C molding and general purpose extrusions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in..
Copyright © lookpolymers.com All Rights Reserved