Axiall 59996J Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 59996J Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.16 - 1.20 g/cc
1.16 - 1.20 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 64
58 - 64
delayed; ASTM D-2240
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D-638
Elongation at Yield 400 %
400 %
ASTM D-638
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -50.0 °C
-58.0 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 168 °C
335 °F