Axiall 16640 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 16640 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Matte finish battery booster cable jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.18 - 1.22 g/cc
1.18 - 1.22 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 61 - 67
61 - 67
delayed; ASTM D-2240
Tensile Strength, Yield 11.7 MPa
1700 psi
ASTM D-638
Elongation at Yield 350 %
350 %
ASTM D-638
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -57.0 °C
-70.6 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F