Material Notes:
Application: RoHS compliant, 105° C, flexible, oil resistant TPE jacketing material with extremely good low temperature properties.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.14 - 1.20 g/cc
1.14 - 1.20 g/cc
ASTM D792
Deformation 63 %

@Temperature 1.00 °C,
Time 540000 sec
63 %

@Temperature 33.8 °F,
Time 150 hour
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 70
58 - 70
ASTM D2240
Tensile Strength 11.8 MPa
1710 psi
ASTM D412
13.2 MPa

@Treatment Temp. 60.0 °C,
Time 605000 sec
1910 psi

@Treatment Temp. 140 °F,
Time 168 hour
Oil #2
14.04 MPa

@Treatment Temp. 136 °C,
Time 605000 sec
2036 psi

@Treatment Temp. 277 °F,
Time 168 hour
Oven
Elongation at Break 350 %
350 %
ASTM D412
297.5 %

@Treatment Temp. 136 °C,
Time 605000 sec
297.5 %

@Treatment Temp. 277 °F,
Time 168 hour
Oven
301 %

@Treatment Temp. 60.0 °C,
Time 605000 sec
301 %

@Treatment Temp. 140 °F,
Time 168 hour
Oil #2
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -53.0 °C
-63.4 °F
ASTM D746
Oxygen Index 26.5 %
26.5 %