Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LD 761.36 Molding, extrusion and compounding resin

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Manufacturer Exxon Chemical
Trade Name Escorene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD 761.36 Molding, extrusion and compounding resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Escorene Ultra LD 761.36 is a 26.7% vinyl acetate copolymer excellent flexibility and low temperature toughness. LD 761.36 has high filler acceptance.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:CompoundingMasterbatch Base ResinProfile ExtrusionTube ExtrusionInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ExxonMobil Method
Vinyl Acetate Content 26.7 %
26.7 %
ExxonMobil Method
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
15s; ASTM D2240
Hardness, Shore D 27
27
15s; ASTM D2240
Tensile Strength at Break 8.27 MPa
1200 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0283 GPa
4.10 ksi
1% secant; ASTM D790
Impact Test 19.0 J

@Temperature 23.0 °C
14.0 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
29.8 J

@Temperature -40.0 °C
22.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
Thermal Properties Metric English Comments
Melting Point 72.8 °C
163 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 46.1 °C
115 °F
ASTM D1525
Descriptive Properties Value Comments
Features Thermal Stabilizer