Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufFill™ 5008 Polyolefin

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer S&E Specialty Polymers
Trade Name TufFill™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFill™ 5008 Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV protection or paintable version.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ISO 1183
Melt Flow 20.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength 17.0 MPa
2470 psi
ISO 527
Flexural Modulus 2.268 GPa
328.9 ksi
ISO 178
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
ISO 180/1A
Impact Test 19.0 J

@Temperature 23.0 °C
14.0 ft-lb

@Temperature 73.4 °F
multiaxial, at 2.2 m/sec, 100% ductile; ASTM 3763
22.4 J

@Temperature -10.0 °C
16.5 ft-lb

@Temperature 14.0 °F
multiaxial, at 2.2 m/sec, 100% ductile; ASTM 3763
Copyright © lookpolymers.com All Rights Reserved