Mechanical Properties Metric English Comments
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group 3536 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group DECAL® 2061 Phenolic
Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and ..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group DECAL® 5431 Phenolic
Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group DECAL® 572R Phenolic
Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group DECAL® 666/8 Phenolic
Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group DECAL® 666/8/2B Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound
Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on ..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very ..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group EPOXIDUR® 3582 EP Epoxy
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group MELOPAS® 156 MF Melamine
Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group MELOPAS® 2010 MF Melamine
Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group MELOPAS® 6605 MP Melamine
Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
Injection and Compression; ISO 604
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group MELOPLAS® 181 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
Injection and Compression; ISO 604
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
Injection and Compression; ISO 604
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group SURAPLAST UPA 63 UP
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
Compressive Strength 220 - 250 MPa
31900 - 36300 psi
ISO 604
Vyncolit 4221 XB Novolac Phenolic
Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group
Compressive Strength 200 - 250 MPa
29000 - 36300 psi
ISO 604
Raschig Group MELOPLAS® 180 MF
Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing ..
Compressive Strength 50.0 - 250 MPa
7250 - 36300 psi
Transverse
Goodfellow Carbon/Epoxy Composite Rod
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.