Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 7250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 50.0 MPa
7250 psi
cured at 725°C, based on ASTM C133-84
Pyrotek Pyrocast 220HT Refractory Castable
Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.ApplicationsTransfer troughs Launder linings Filter boxes Pins and spouts AdvantagesThermal shock r..
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Gouda Vuurvast AK 42 Dense Refractory Brick
Description: Because of its abrasion resistance and high density, this brick performs very well in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were c..
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Gouda Vuurvast AK 46 S Dense Refractory Brick
Description: AK 46 S is a very dense, high quality firebrick with low iron and alkali content, characterized by a low creep (after 24 hours at 1280°C at a load of 0.2 MPa, the creep is only 0.05%..
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Gouda Vuurvast AK 50 Dense Refractory Brick
Description: This brick has a low iron and alkali content and is therefore suitable for use in reducing atmospheres at high temperatures. Very good resistance to slag attack. Application: incinerato..
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Gouda Vuurvast AK 53 E Dense Refractory Brick
Description: Because of its very high erosion resistance this brick is applied in e.g. recirculation cyclones for CFB coal fired boilers.Remarks: This data represents average values, obtained from s..
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Gouda Vuurvast AK 80 Dense Refractory Brick
Description: A bauxite based quality with a high abrasion resistance. Widely used in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were cut from standa..
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Gouda Vuurvast AK 80 FM Dense Refractory Brick
Description: This fused mullite based brick has a very good thermal shock resistance and an excellent resistance against liquid slags at high temperature.Remarks: This data represents average values..
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Gouda Vuurvast AK 60 C Dense Refractory Brick
Description: A bauxite based quality with a high abrasion resistance, successfully used in transition zones of rotary cement kilns.Remarks: This data represents average values, obtained from samples..
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Gouda Vuurvast C Sp Dense Refractory Brick
Description: A fireclay brick for use up to 1200°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Compressive Strength 50.0 MPa
7250 psi
5% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene
Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 50.0 MPa
7250 psi
EN 993-5 1998
Skamol Group SKAMOBAR 69 Low-Alumina Fireclay Brick
Low-alumina fireclay brick has the following characteristics: Max. service temperature 1100°C (2012°F)For barrier lining of aluminum reduction cellsExcellent cryolite resistanceLow thermal con..
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Chosun Refractories A8S Magnesia Carbon Bricks for Electric Arc Furnace
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Chosun Refractories AB10H Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Chosun Refractories AB10L Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Chosun Refractories AB10S Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Chosun Refractories AM10H Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Chosun Refractories AM10S Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Chosun Refractories AMC-65 Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Chosun Refractories AMC-70 Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Chosun Refractories ASC-S Alumina Silicon Carbide Carbon Bricks for Torpedo Car
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength >= 50.0 MPa
>= 7250 psi
Axial; IEC 1212-2 5.3
Hippe SI MP 21 Mica Paper Reinforced Silicone Resin - Round, Rolled Tube
Used in mechanical, electrical and electronic applications. Good stability of electrical properties at elevated temperatures.Information provided by Hippe.
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Chosun Refractories L8S Magnesia Carbon Bricks for Ladle Slag Line
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Chosun Refractories AM10L Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 50.0 - 250 MPa
7250 - 36300 psi
Transverse
Goodfellow Carbon/Epoxy Composite Rod
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Gouda Vuurvast AK 50 A Dense Refractory Brick
Description: This brick has a low porosity and a high strength and therefore a very good slag resistance. Applications: rotary cement kilns.Remarks: This data represents average values, obtained fro..
Copyright © lookpolymers.com All Rights Reserved