Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 50.0 MPa | 7250 psi | cured at 725°C, based on ASTM C133-84 |
Pyrotek Pyrocast 220HT Refractory Castable Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.ApplicationsTransfer troughs Launder linings Filter boxes Pins and spouts AdvantagesThermal shock r.. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Gouda Vuurvast AK 42 Dense Refractory Brick Description: Because of its abrasion resistance and high density, this brick performs very well in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were c.. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Gouda Vuurvast AK 46 S Dense Refractory Brick Description: AK 46 S is a very dense, high quality firebrick with low iron and alkali content, characterized by a low creep (after 24 hours at 1280°C at a load of 0.2 MPa, the creep is only 0.05%.. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Gouda Vuurvast AK 50 Dense Refractory Brick Description: This brick has a low iron and alkali content and is therefore suitable for use in reducing atmospheres at high temperatures. Very good resistance to slag attack. Application: incinerato.. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Gouda Vuurvast AK 53 E Dense Refractory Brick Description: Because of its very high erosion resistance this brick is applied in e.g. recirculation cyclones for CFB coal fired boilers.Remarks: This data represents average values, obtained from s.. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Gouda Vuurvast AK 80 Dense Refractory Brick Description: A bauxite based quality with a high abrasion resistance. Widely used in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were cut from standa.. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Gouda Vuurvast AK 80 FM Dense Refractory Brick Description: This fused mullite based brick has a very good thermal shock resistance and an excellent resistance against liquid slags at high temperature.Remarks: This data represents average values.. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Gouda Vuurvast AK 60 C Dense Refractory Brick Description: A bauxite based quality with a high abrasion resistance, successfully used in transition zones of rotary cement kilns.Remarks: This data represents average values, obtained from samples.. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Gouda Vuurvast C Sp Dense Refractory Brick Description: A fireclay brick for use up to 1200°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | 5% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 50.0 MPa | 7250 psi | EN 993-5 1998 |
Skamol Group SKAMOBAR 69 Low-Alumina Fireclay Brick Low-alumina fireclay brick has the following characteristics: Max. service temperature 1100°C (2012°F)For barrier lining of aluminum reduction cellsExcellent cryolite resistanceLow thermal con.. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Chosun Refractories A8S Magnesia Carbon Bricks for Electric Arc Furnace Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Chosun Refractories AB10H Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Chosun Refractories AB10L Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Chosun Refractories AB10S Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Chosun Refractories AM10H Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Chosun Refractories AM10S Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Chosun Refractories AMC-65 Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Chosun Refractories AMC-70 Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Chosun Refractories ASC-S Alumina Silicon Carbide Carbon Bricks for Torpedo Car Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | >= 50.0 MPa | >= 7250 psi | Axial; IEC 1212-2 5.3 |
Hippe SI MP 21 Mica Paper Reinforced Silicone Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Good stability of electrical properties at elevated temperatures.Information provided by Hippe. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Chosun Refractories L8S Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Chosun Refractories AM10L Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 50.0 - 250 MPa | 7250 - 36300 psi | Transverse |
Goodfellow Carbon/Epoxy Composite Rod Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |
|||
Compressive Strength | 50.0 MPa | 7250 psi | Cold Crushing Strength |
Gouda Vuurvast AK 50 A Dense Refractory Brick Description: This brick has a low porosity and a high strength and therefore a very good slag resistance. Applications: rotary cement kilns.Remarks: This data represents average values, obtained fro.. |