Goodfellow Carbon/Epoxy Composite Rod

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Goodfellow
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Carbon/Epoxy Composite Rod.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
Transverse
1100 - 1900 MPa
160000 - 276000 psi
Longitudinal
Elongation at Break 0.50 %
0.50 %
Transverse - Tensile
0.80 %
0.80 %
Longitudinal Compressive Strain
1.1 %
1.1 %
Longitudinal - Tensile
2.5 %
2.5 %
Transverse Compressive Strain
Modulus of Elasticity 10.0 GPa
1450 ksi
Transverse
Tensile Modulus 120 - 140 GPa
17400 - 20300 ksi
Longitudinal
Flexural Strength 1200 MPa
174000 psi
Longitudinal
Flexural Modulus 125 GPa
18100 ksi
Longitudinal
Compressive Strength 50.0 - 250 MPa
7250 - 36300 psi
Transverse
800 - 1300 MPa
116000 - 189000 psi
Longitudinal
Thermal Properties Metric English Comments
CTE, linear -0.700 - -0.300 µm/m-°C

@Temperature 20.0 °C
-0.389 - -0.167 µin/in-°F

@Temperature 68.0 °F
Longitudinal
CTE, linear, Transverse to Flow 28.0 µm/m-°C

@Temperature 20.0 °C
15.6 µin/in-°F

@Temperature 68.0 °F
Descriptive Properties Value Comments
Volume Fraction Fibers, % 55-60