Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | Deflection @ 25%; ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ C43 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ C43NBR Nitrile Rubber Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | Deflection @ 25% |
Monmouth Rubber & Plastics Durafoamâ„¢ DK3131 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ P391SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ P392SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ P493SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ P497SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Compressive Strength | 0.0621 - 0.0965 MPa | 9.00 - 14.0 psi | 0.25; ASTM D1056 |
Monmouth Rubber & Plastics Superbounce 57 NEO/SBR Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0621 MPa | 9.00 psi | Compression Deflection, Value given for 12.7 mm/min, 25% deflection.; ASTM D3574 Test C |
Saint-Gobain Korel® K40-30 Medium Deflection Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Compressive Strength | 0.0621 MPa | 9.00 psi | Method A, 22 hrs @ 158°F under 1350 psi |
Tra-Con Tra-Bond Ablebond 724-1 Polyurethane Adhesive Ablebond 724-1 premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates.Information provided by Tra-Con Inc. |