Polymer Property : Compressive Strength = 9.00 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
Deflection @ 25%; ASTM D1056
Monmouth Rubber & Plastics Durafoamâ„¢ C43 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ C43NBR Nitrile Rubber
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
Deflection @ 25%
Monmouth Rubber & Plastics Durafoamâ„¢ DK3131 NEO/EPDM Polymeric Blend
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ P391SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ P392SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ P493SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ P497SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Compressive Strength 0.0621 - 0.0965 MPa
9.00 - 14.0 psi
0.25; ASTM D1056
Monmouth Rubber & Plastics Superbounce 57 NEO/SBR
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0621 MPa
9.00 psi
Compression Deflection, Value given for 12.7 mm/min, 25% deflection.; ASTM D3574 Test C
Saint-Gobain Korel® K40-30 Medium Deflection Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi..
Compressive Strength 0.0621 MPa
9.00 psi
Method A, 22 hrs @ 158°F under 1350 psi
Tra-Con Tra-Bond Ablebond 724-1 Polyurethane Adhesive
Ablebond 724-1 premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates.Information provided by Tra-Con Inc.
Copyright © lookpolymers.com All Rights Reserved