Polymer Property : Compressive Strength = 13.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
Deflection @ 25%; ASTM D1056
Monmouth Rubber & Plastics Durafoamâ„¢ C43 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ C43NBR Nitrile Rubber
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
Deflection @ 25%
Monmouth Rubber & Plastics Durafoamâ„¢ DK3131 NEO/EPDM Polymeric Blend
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0345 - 0.0896 MPa
5.00 - 13.0 psi
Deflection @ 25%; ASTM D1056
Monmouth Rubber & Plastics Durafoamâ„¢ N207 100% Neoprene
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ P391SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ P392SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ P493SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Compressive Strength 0.0621 - 0.0896 MPa
9.00 - 13.0 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ P497SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..