Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | Deflection @ 25%; ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ C43 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ C43NBR Nitrile Rubber Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | Deflection @ 25% |
Monmouth Rubber & Plastics Durafoamâ„¢ DK3131 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0345 - 0.0896 MPa | 5.00 - 13.0 psi | Deflection @ 25%; ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ N207 100% Neoprene Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ P391SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ P392SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ P493SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Compressive Strength | 0.0621 - 0.0896 MPa | 9.00 - 13.0 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ P497SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |