Material Notes:
Information provided by Monmouth Rubber & Plastics Corp.
Physical Properties Metric English Comments
Density >= 0.224 g/cc
>= 0.00810 lb/in³
Water Absorption <= 2.0 %
<= 2.0 %
ASTM D1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 56 - 62
56 - 62
ASTM D2240
Tensile Strength 1.31 MPa
190 psi
ASTM D2000
Elongation at Break 250 %
250 %
ASTM D2000
Compressive Strength 0.0621 - 0.0965 MPa
9.00 - 14.0 psi
0.25; ASTM D1056
0.186 - 0.228 MPa
27.0 - 33.0 psi
0.5; ASTM D1056
Tear Strength 3.51 kN/m
20.0 pli
Die C; ASTM D3575 Suf. G
Compression Set 5.0 %

@Time 86400 sec
5.0 %

@Time 24.0 hour
8.0 %

@Time 3600 sec
8.0 %

@Time 1.00 hour
12 %

@Time 299 sec
12 %

@Time 0.0830 hour
13 %

@Time 60.0 sec
13 %

@Time 0.0167 hour
18 %

@Time 5.00 sec
18 %

@Time 0.00139 hour
Descriptive Properties Value Comments
C/D Heat Aging 0.3
7 days @158°F, Change; ASTM D1056
Color Black
Compression Recovery 0.89
5 sec; ASTM D1056
0.9
60 sec; ASTM D1056
0.94
5 mins; ASTM D1056
0.94
60 mins; ASTM D1056
0.95
24 hrs; ASTM D1056